Ni Cr Fe based alloy superalloy

Ni Cr Fe based alloy superalloy
Product Detailed
Ni Cr Fe based superalloy 1)good quality with price and technical advantages 2)service quickly and in time 3)have experiences

Ni Cr Fe based superalloy1)good quality with price and technical advantages2)service quickly and in time3)have experiences

ASTM B603, DIN 17470, JIS C2520, GB/T1234.

Our advantage:High quality,short delivery time,small MOQ.

A superalloy, or high-performance alloy, is an alloy that exhibits excellent mechanical strength and creep resistance at high temperatures, good surface stability, and corrosion and oxidation resistance. Superalloys typically have a matrix with an austenitic face-centered cubic crystal structure. A superalloy's base alloying element is usually nickel, cobalt, or nickel-iron. Inconel, Hastelloy

Usage:Resistance heating elements;Material in metallurgy;Household appliances;Mechanical manufacturing and other industries.

for further information, please do not hestitate to contact us.